Abstract

A device was developed for the continuous measurement of the open circuit corrosion rate of aluminum in deaerated water from hydrogen pressure, resulted from the cathodic reaction. Corrosion rate of aluminum coated by the passive oxide film was examined with respect to the corrosion phenomena using this device. From the results, it was found that the corrosion rate was dependent not only on the deterioration of the film, but also on the formation of pits and of corrosion products on the film. Furthermore, the deterioration of the film was independent on the pH of the water. The pits were most probably formed by the evolution of hydrogen gas at the cathode underneath the film followed by the formation of Al (OH)4-.

Original languageEnglish
Pages (from-to)2581-2601
Number of pages21
JournalCorrosion Science
Volume49
Issue number6
DOIs
Publication statusPublished - Jun 1 2007

Fingerprint

Aluminum corrosion
Corrosion rate
Water
Monitoring
Aluminum
Deterioration
Hydrogen
Corrosion
Oxide films
Cathodes
Gases
Networks (circuits)

All Science Journal Classification (ASJC) codes

  • Chemistry(all)
  • Chemical Engineering(all)
  • Materials Science(all)

Cite this

Continuous monitoring of aluminum corrosion process in deaerated water. / Ishii, Katsuya; Ozaki, Ryota; Kaneko, Kenji; Fukushima, Hisaaki; Masuda, Masataka.

In: Corrosion Science, Vol. 49, No. 6, 01.06.2007, p. 2581-2601.

Research output: Contribution to journalArticle

Ishii, Katsuya ; Ozaki, Ryota ; Kaneko, Kenji ; Fukushima, Hisaaki ; Masuda, Masataka. / Continuous monitoring of aluminum corrosion process in deaerated water. In: Corrosion Science. 2007 ; Vol. 49, No. 6. pp. 2581-2601.
@article{6ab903c848d8445c9cb3ee675b18476b,
title = "Continuous monitoring of aluminum corrosion process in deaerated water",
abstract = "A device was developed for the continuous measurement of the open circuit corrosion rate of aluminum in deaerated water from hydrogen pressure, resulted from the cathodic reaction. Corrosion rate of aluminum coated by the passive oxide film was examined with respect to the corrosion phenomena using this device. From the results, it was found that the corrosion rate was dependent not only on the deterioration of the film, but also on the formation of pits and of corrosion products on the film. Furthermore, the deterioration of the film was independent on the pH of the water. The pits were most probably formed by the evolution of hydrogen gas at the cathode underneath the film followed by the formation of Al (OH)4-.",
author = "Katsuya Ishii and Ryota Ozaki and Kenji Kaneko and Hisaaki Fukushima and Masataka Masuda",
year = "2007",
month = "6",
day = "1",
doi = "10.1016/j.corsci.2006.12.015",
language = "English",
volume = "49",
pages = "2581--2601",
journal = "Corrosion Science",
issn = "0010-938X",
publisher = "Elsevier Limited",
number = "6",

}

TY - JOUR

T1 - Continuous monitoring of aluminum corrosion process in deaerated water

AU - Ishii, Katsuya

AU - Ozaki, Ryota

AU - Kaneko, Kenji

AU - Fukushima, Hisaaki

AU - Masuda, Masataka

PY - 2007/6/1

Y1 - 2007/6/1

N2 - A device was developed for the continuous measurement of the open circuit corrosion rate of aluminum in deaerated water from hydrogen pressure, resulted from the cathodic reaction. Corrosion rate of aluminum coated by the passive oxide film was examined with respect to the corrosion phenomena using this device. From the results, it was found that the corrosion rate was dependent not only on the deterioration of the film, but also on the formation of pits and of corrosion products on the film. Furthermore, the deterioration of the film was independent on the pH of the water. The pits were most probably formed by the evolution of hydrogen gas at the cathode underneath the film followed by the formation of Al (OH)4-.

AB - A device was developed for the continuous measurement of the open circuit corrosion rate of aluminum in deaerated water from hydrogen pressure, resulted from the cathodic reaction. Corrosion rate of aluminum coated by the passive oxide film was examined with respect to the corrosion phenomena using this device. From the results, it was found that the corrosion rate was dependent not only on the deterioration of the film, but also on the formation of pits and of corrosion products on the film. Furthermore, the deterioration of the film was independent on the pH of the water. The pits were most probably formed by the evolution of hydrogen gas at the cathode underneath the film followed by the formation of Al (OH)4-.

UR - http://www.scopus.com/inward/record.url?scp=34047254296&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=34047254296&partnerID=8YFLogxK

U2 - 10.1016/j.corsci.2006.12.015

DO - 10.1016/j.corsci.2006.12.015

M3 - Article

AN - SCOPUS:34047254296

VL - 49

SP - 2581

EP - 2601

JO - Corrosion Science

JF - Corrosion Science

SN - 0010-938X

IS - 6

ER -