N2 - Anatase of good crystallinity has been developed on titanium substrates by soaking in a 30 mass% hydrogen peroxide solution at 80°C for 8 h, soaking in distilled water at ambient temperature for 12 h, and subsequently aging in distilled water at 80°C for 3d. The anatase layers exhibit good bioactivity as inducing apatite deposition in Kokubo's simulated body fluid within 2d.
AB - Anatase of good crystallinity has been developed on titanium substrates by soaking in a 30 mass% hydrogen peroxide solution at 80°C for 8 h, soaking in distilled water at ambient temperature for 12 h, and subsequently aging in distilled water at 80°C for 3d. The anatase layers exhibit good bioactivity as inducing apatite deposition in Kokubo's simulated body fluid within 2d.
UR - http://www.scopus.com/inward/record.url?scp=0002690858&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=0002690858&partnerID=8YFLogxK
U2 - 10.2109/jcersj.110.78
DO - 10.2109/jcersj.110.78
M3 - Article
AN - SCOPUS:0002690858
SN - 1882-0743
VL - 110
SP - 78
EP - 80
JO - Nippon Seramikkusu Kyokai Gakujutsu Ronbunshi/Journal of the Ceramic Society of Japan
JF - Nippon Seramikkusu Kyokai Gakujutsu Ronbunshi/Journal of the Ceramic Society of Japan
IS - 1278
ER -