Differential scanning calorimetry measurements of magnesium borohydride Mg(BH4)2

Yigang Yan, Hai Wen Li, Yuko Nakamori, Nobuko Ohba Kazutoshi Miwa, Shin Ichi Towata, Shin Ichi Orimo

Research output: Contribution to journalArticlepeer-review

24 Citations (Scopus)

Abstract

Multistep dehydriding reactions of magnesium borohydride Mg(BH 4)2 were studied by Differential Scanning Calorimetry (DSC) measurements. The values of the enthalpy changes of the reactions from the measurements are in good agreement with those from first-principles calculations. Kinetically restricted dehydriding reaction of Mg(BH 4)2, suggested also by the measurements, was briefly discussed.

Original languageEnglish
Pages (from-to)2751-2752
Number of pages2
JournalMaterials Transactions
Volume49
Issue number11
DOIs
Publication statusPublished - Nov 1 2008
Externally publishedYes

All Science Journal Classification (ASJC) codes

  • Materials Science(all)
  • Condensed Matter Physics
  • Mechanics of Materials
  • Mechanical Engineering

Fingerprint

Dive into the research topics of 'Differential scanning calorimetry measurements of magnesium borohydride Mg(BH4)2'. Together they form a unique fingerprint.

Cite this