Effect of isothermal heat treatment on nanoindentation hardness and Young's modulus of 4 mol% Y2O3-ZrO2 EB-PVD TBCs

Byung Koog Jang, Seung Hyeon Kim, Craig A.J. Fisher, Hyung Tae Kim

Research output: Contribution to journalArticlepeer-review

3 Citations (Scopus)

Fingerprint

Dive into the research topics of 'Effect of isothermal heat treatment on nanoindentation hardness and Young's modulus of 4 mol% Y2O3-ZrO2 EB-PVD TBCs'. Together they form a unique fingerprint.

Material Science