Effect of post-calcination thermal treatment on acid properties and pores structure of a mesoporous niobium-tungsten oxide was examined. Mesoporous Nb-W oxides treated by high temperature calcination from 673 up to 873 K exhibited a significant increase in pore size from 4.8 to 9.2 nm, a decrease in pore volume, surface area and acid amount, while the acid strength and density remained almost constant. A remarkable improvement in acid catalysis was observed for Friedel-Crafts alkylation and hydrolysis of disaccharide where the turnover frequency for both reactions increased continuously with calcination temperature.

Original languageEnglish
Pages (from-to)144-148
Number of pages5
JournalCatalysis Today
Volume192
Issue number1
DOIs
Publication statusPublished - Sep 30 2012
Externally publishedYes

Fingerprint

Niobium
Pore structure
Calcination
Tungsten
Heat treatment
Acids
Oxides
Disaccharides
Alkylation
Catalysis
Pore size
Hydrolysis
Temperature
tungsten oxide

All Science Journal Classification (ASJC) codes

  • Catalysis
  • Chemistry(all)

Cite this

Effect of post-calcination thermal treatment on acid properties and pores structure of a mesoporous niobium-tungsten oxide. / Takagaki, Atsushi; Tagusagawa, Caio; Takanabe, Kazuhiro; Kondo, Junko N.; Tatsumi, Takashi; Domen, Kazunari.

In: Catalysis Today, Vol. 192, No. 1, 30.09.2012, p. 144-148.

Research output: Contribution to journalArticle

Takagaki, Atsushi ; Tagusagawa, Caio ; Takanabe, Kazuhiro ; Kondo, Junko N. ; Tatsumi, Takashi ; Domen, Kazunari. / Effect of post-calcination thermal treatment on acid properties and pores structure of a mesoporous niobium-tungsten oxide. In: Catalysis Today. 2012 ; Vol. 192, No. 1. pp. 144-148.
@article{5f8e99927d07406fb288a101ff4b8aae,
title = "Effect of post-calcination thermal treatment on acid properties and pores structure of a mesoporous niobium-tungsten oxide",
abstract = "Effect of post-calcination thermal treatment on acid properties and pores structure of a mesoporous niobium-tungsten oxide was examined. Mesoporous Nb-W oxides treated by high temperature calcination from 673 up to 873 K exhibited a significant increase in pore size from 4.8 to 9.2 nm, a decrease in pore volume, surface area and acid amount, while the acid strength and density remained almost constant. A remarkable improvement in acid catalysis was observed for Friedel-Crafts alkylation and hydrolysis of disaccharide where the turnover frequency for both reactions increased continuously with calcination temperature.",
author = "Atsushi Takagaki and Caio Tagusagawa and Kazuhiro Takanabe and Kondo, {Junko N.} and Takashi Tatsumi and Kazunari Domen",
year = "2012",
month = "9",
day = "30",
doi = "10.1016/j.cattod.2011.11.036",
language = "English",
volume = "192",
pages = "144--148",
journal = "Catalysis Today",
issn = "0920-5861",
publisher = "Elsevier",
number = "1",

}

TY - JOUR

T1 - Effect of post-calcination thermal treatment on acid properties and pores structure of a mesoporous niobium-tungsten oxide

AU - Takagaki, Atsushi

AU - Tagusagawa, Caio

AU - Takanabe, Kazuhiro

AU - Kondo, Junko N.

AU - Tatsumi, Takashi

AU - Domen, Kazunari

PY - 2012/9/30

Y1 - 2012/9/30

N2 - Effect of post-calcination thermal treatment on acid properties and pores structure of a mesoporous niobium-tungsten oxide was examined. Mesoporous Nb-W oxides treated by high temperature calcination from 673 up to 873 K exhibited a significant increase in pore size from 4.8 to 9.2 nm, a decrease in pore volume, surface area and acid amount, while the acid strength and density remained almost constant. A remarkable improvement in acid catalysis was observed for Friedel-Crafts alkylation and hydrolysis of disaccharide where the turnover frequency for both reactions increased continuously with calcination temperature.

AB - Effect of post-calcination thermal treatment on acid properties and pores structure of a mesoporous niobium-tungsten oxide was examined. Mesoporous Nb-W oxides treated by high temperature calcination from 673 up to 873 K exhibited a significant increase in pore size from 4.8 to 9.2 nm, a decrease in pore volume, surface area and acid amount, while the acid strength and density remained almost constant. A remarkable improvement in acid catalysis was observed for Friedel-Crafts alkylation and hydrolysis of disaccharide where the turnover frequency for both reactions increased continuously with calcination temperature.

UR - http://www.scopus.com/inward/record.url?scp=84866089278&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84866089278&partnerID=8YFLogxK

U2 - 10.1016/j.cattod.2011.11.036

DO - 10.1016/j.cattod.2011.11.036

M3 - Article

AN - SCOPUS:84866089278

VL - 192

SP - 144

EP - 148

JO - Catalysis Today

JF - Catalysis Today

SN - 0920-5861

IS - 1

ER -