Fatigue behaviour of out-of-plane gusset joints with one-side fillet weld

Shigenobu Kainuma, Kini To, Daisuke Uchida, Nobuaki Yagi, Hiroshi Kubo

Research output: Contribution to journalArticle

Abstract

In previous studies, many fatigue tests have been performed to investigate the fatigue behaviour of out-of-plane gusset welded joints. However, fatigue behaviour of out-of-plane gusset joints with a one-side fillet weld has not yet been clarified sufficiently. In this research, in order to quantitatively clarify the behaviour, welding residual stress at the weld toes of the joint was measured by a cutting method. In addition to this, fatigue tests were carried out on the joints with a one-side weld and turn-around weld. The plate thickness is 9 mm and the weld size is 10 mm. Moreover, finite element stress analyses were conducted on the test specimen models and parametric models with different main plate and gusset plate thickness. Their results show that fatigue cracks for out-of-plane gusset joints with a one-side fillet weld initiate from both weld toes at the start and end points of weld beads and non-penetration weld of the gusset side. Also, the crack initiation points are different depending on the weld arrangement; however, their fatigue strengths are almost same.

Original languageEnglish
Pages (from-to)913-921
Number of pages9
JournalWelding International
Volume29
Issue number12
DOIs
Publication statusPublished - Dec 2 2015

Fingerprint

Welds
Fatigue of materials
Crack initiation
Residual stresses
Welding

All Science Journal Classification (ASJC) codes

  • Mechanics of Materials
  • Mechanical Engineering
  • Metals and Alloys

Cite this

Fatigue behaviour of out-of-plane gusset joints with one-side fillet weld. / Kainuma, Shigenobu; To, Kini; Uchida, Daisuke; Yagi, Nobuaki; Kubo, Hiroshi.

In: Welding International, Vol. 29, No. 12, 02.12.2015, p. 913-921.

Research output: Contribution to journalArticle

Kainuma, Shigenobu ; To, Kini ; Uchida, Daisuke ; Yagi, Nobuaki ; Kubo, Hiroshi. / Fatigue behaviour of out-of-plane gusset joints with one-side fillet weld. In: Welding International. 2015 ; Vol. 29, No. 12. pp. 913-921.
@article{0864b49a157a426aad2aaf59e1d7abe8,
title = "Fatigue behaviour of out-of-plane gusset joints with one-side fillet weld",
abstract = "In previous studies, many fatigue tests have been performed to investigate the fatigue behaviour of out-of-plane gusset welded joints. However, fatigue behaviour of out-of-plane gusset joints with a one-side fillet weld has not yet been clarified sufficiently. In this research, in order to quantitatively clarify the behaviour, welding residual stress at the weld toes of the joint was measured by a cutting method. In addition to this, fatigue tests were carried out on the joints with a one-side weld and turn-around weld. The plate thickness is 9 mm and the weld size is 10 mm. Moreover, finite element stress analyses were conducted on the test specimen models and parametric models with different main plate and gusset plate thickness. Their results show that fatigue cracks for out-of-plane gusset joints with a one-side fillet weld initiate from both weld toes at the start and end points of weld beads and non-penetration weld of the gusset side. Also, the crack initiation points are different depending on the weld arrangement; however, their fatigue strengths are almost same.",
author = "Shigenobu Kainuma and Kini To and Daisuke Uchida and Nobuaki Yagi and Hiroshi Kubo",
year = "2015",
month = "12",
day = "2",
doi = "10.1080/09507116.2014.921082",
language = "English",
volume = "29",
pages = "913--921",
journal = "Welding International",
issn = "0950-7116",
publisher = "Taylor and Francis Ltd.",
number = "12",

}

TY - JOUR

T1 - Fatigue behaviour of out-of-plane gusset joints with one-side fillet weld

AU - Kainuma, Shigenobu

AU - To, Kini

AU - Uchida, Daisuke

AU - Yagi, Nobuaki

AU - Kubo, Hiroshi

PY - 2015/12/2

Y1 - 2015/12/2

N2 - In previous studies, many fatigue tests have been performed to investigate the fatigue behaviour of out-of-plane gusset welded joints. However, fatigue behaviour of out-of-plane gusset joints with a one-side fillet weld has not yet been clarified sufficiently. In this research, in order to quantitatively clarify the behaviour, welding residual stress at the weld toes of the joint was measured by a cutting method. In addition to this, fatigue tests were carried out on the joints with a one-side weld and turn-around weld. The plate thickness is 9 mm and the weld size is 10 mm. Moreover, finite element stress analyses were conducted on the test specimen models and parametric models with different main plate and gusset plate thickness. Their results show that fatigue cracks for out-of-plane gusset joints with a one-side fillet weld initiate from both weld toes at the start and end points of weld beads and non-penetration weld of the gusset side. Also, the crack initiation points are different depending on the weld arrangement; however, their fatigue strengths are almost same.

AB - In previous studies, many fatigue tests have been performed to investigate the fatigue behaviour of out-of-plane gusset welded joints. However, fatigue behaviour of out-of-plane gusset joints with a one-side fillet weld has not yet been clarified sufficiently. In this research, in order to quantitatively clarify the behaviour, welding residual stress at the weld toes of the joint was measured by a cutting method. In addition to this, fatigue tests were carried out on the joints with a one-side weld and turn-around weld. The plate thickness is 9 mm and the weld size is 10 mm. Moreover, finite element stress analyses were conducted on the test specimen models and parametric models with different main plate and gusset plate thickness. Their results show that fatigue cracks for out-of-plane gusset joints with a one-side fillet weld initiate from both weld toes at the start and end points of weld beads and non-penetration weld of the gusset side. Also, the crack initiation points are different depending on the weld arrangement; however, their fatigue strengths are almost same.

UR - http://www.scopus.com/inward/record.url?scp=84930820352&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84930820352&partnerID=8YFLogxK

U2 - 10.1080/09507116.2014.921082

DO - 10.1080/09507116.2014.921082

M3 - Article

VL - 29

SP - 913

EP - 921

JO - Welding International

JF - Welding International

SN - 0950-7116

IS - 12

ER -