Gold refining by cementation with salt at Sado in early seventeenth century Japan

Eiji Izawa, Tetsuya Nakanishi

Research output: Contribution to journalArticle

Abstract

In the seventeenth century Japanese gold production became the highest rank of the world and Sado gold contributed nearly half to the domestic production. The key technology of massive gold production was gold-silver parting by cementation process with salt. During the excavation of the Sado Bugyosho (magistrate office) site, in 1996, gold refining remains were found below the 1647 fire horizon. A total of 29 furnaces were found in an area of east-west 17 m by north-south 8 m. The largest furnace is an elongated shallow tray-like furnace, which resembles closely the cementation furnace illustrated in eighteenthand nineteenth-century picture scrolls of the mine. Large number of fragments of earthenware such as clay dishes, clay plates and clay rods were unearthed. Many of the earthenware were discolored from the original reddish color. The chemical compositions of discolored samples are characterized by increase in Na2O, K2O, S, Cl and Ag, and decrease in SiO2 and Fe2O3 indicating the gold-silver parting reaction by common salt.

Original languageEnglish
Pages (from-to)1098-1105
Number of pages8
Journalisij international
Volume54
Issue number5
DOIs
Publication statusPublished - Jan 1 2014

Fingerprint

Gold refining
Gold
Salts
Furnaces
Clay
Silver
Excavation
Fires
Color
Chemical analysis

All Science Journal Classification (ASJC) codes

  • Mechanics of Materials
  • Mechanical Engineering
  • Metals and Alloys
  • Materials Chemistry

Cite this

Gold refining by cementation with salt at Sado in early seventeenth century Japan. / Izawa, Eiji; Nakanishi, Tetsuya.

In: isij international, Vol. 54, No. 5, 01.01.2014, p. 1098-1105.

Research output: Contribution to journalArticle

@article{f21ff0fe2ea44cf187e5bcbdc328dbac,
title = "Gold refining by cementation with salt at Sado in early seventeenth century Japan",
abstract = "In the seventeenth century Japanese gold production became the highest rank of the world and Sado gold contributed nearly half to the domestic production. The key technology of massive gold production was gold-silver parting by cementation process with salt. During the excavation of the Sado Bugyosho (magistrate office) site, in 1996, gold refining remains were found below the 1647 fire horizon. A total of 29 furnaces were found in an area of east-west 17 m by north-south 8 m. The largest furnace is an elongated shallow tray-like furnace, which resembles closely the cementation furnace illustrated in eighteenthand nineteenth-century picture scrolls of the mine. Large number of fragments of earthenware such as clay dishes, clay plates and clay rods were unearthed. Many of the earthenware were discolored from the original reddish color. The chemical compositions of discolored samples are characterized by increase in Na2O, K2O, S, Cl and Ag, and decrease in SiO2 and Fe2O3 indicating the gold-silver parting reaction by common salt.",
author = "Eiji Izawa and Tetsuya Nakanishi",
year = "2014",
month = "1",
day = "1",
doi = "10.2355/isijinternational.54.1098",
language = "English",
volume = "54",
pages = "1098--1105",
journal = "ISIJ International",
issn = "0915-1559",
publisher = "Iron and Steel Institute of Japan",
number = "5",

}

TY - JOUR

T1 - Gold refining by cementation with salt at Sado in early seventeenth century Japan

AU - Izawa, Eiji

AU - Nakanishi, Tetsuya

PY - 2014/1/1

Y1 - 2014/1/1

N2 - In the seventeenth century Japanese gold production became the highest rank of the world and Sado gold contributed nearly half to the domestic production. The key technology of massive gold production was gold-silver parting by cementation process with salt. During the excavation of the Sado Bugyosho (magistrate office) site, in 1996, gold refining remains were found below the 1647 fire horizon. A total of 29 furnaces were found in an area of east-west 17 m by north-south 8 m. The largest furnace is an elongated shallow tray-like furnace, which resembles closely the cementation furnace illustrated in eighteenthand nineteenth-century picture scrolls of the mine. Large number of fragments of earthenware such as clay dishes, clay plates and clay rods were unearthed. Many of the earthenware were discolored from the original reddish color. The chemical compositions of discolored samples are characterized by increase in Na2O, K2O, S, Cl and Ag, and decrease in SiO2 and Fe2O3 indicating the gold-silver parting reaction by common salt.

AB - In the seventeenth century Japanese gold production became the highest rank of the world and Sado gold contributed nearly half to the domestic production. The key technology of massive gold production was gold-silver parting by cementation process with salt. During the excavation of the Sado Bugyosho (magistrate office) site, in 1996, gold refining remains were found below the 1647 fire horizon. A total of 29 furnaces were found in an area of east-west 17 m by north-south 8 m. The largest furnace is an elongated shallow tray-like furnace, which resembles closely the cementation furnace illustrated in eighteenthand nineteenth-century picture scrolls of the mine. Large number of fragments of earthenware such as clay dishes, clay plates and clay rods were unearthed. Many of the earthenware were discolored from the original reddish color. The chemical compositions of discolored samples are characterized by increase in Na2O, K2O, S, Cl and Ag, and decrease in SiO2 and Fe2O3 indicating the gold-silver parting reaction by common salt.

UR - http://www.scopus.com/inward/record.url?scp=84903162793&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84903162793&partnerID=8YFLogxK

U2 - 10.2355/isijinternational.54.1098

DO - 10.2355/isijinternational.54.1098

M3 - Article

VL - 54

SP - 1098

EP - 1105

JO - ISIJ International

JF - ISIJ International

SN - 0915-1559

IS - 5

ER -