Initial stability of a highly porous titanium cup in an acetabular bone defect model

Kensei Yoshimoto, Yasuharu Nakashima, Miyo Wakiyama, Daisuke Hara, Akihiro Nakamura, Mikio Iwamoto

Research output: Contribution to journalArticle

1 Citation (Scopus)

Abstract

Backgrounds: The purpose of this study was to quantify the initial stability of a highly porous titanium cup using an acetabular bone defect model. Methods: The maximum torque of a highly porous titanium cup, with a pore size of 640 μm and porosity of 60%, was measured using rotational and lever-out torque testing and compared to that of a titanium-sprayed cup. The bone models were prepared using a polyurethane foam block and had three levels of bone coverage: 100, 70, and 50%. Results: The highly porous titanium cup demonstrated significantly higher maximum torque than the titanium-sprayed cups in the three levels of bone defects. On rotational torque testing, it was found to be 1.5, 1.3, and 1.3 times stronger than the titanium-sprayed cups with 100, 70 and 50% bone coverage, respectively. Furthermore, it was found to be 2.2, 2.3, and 1.5 times stronger on lever-out testing than the titanium-sprayed cup. No breakage in the porous layers was noted during the testing. Conclusion: This study provides additional evidence of the initial stability of highly porous titanium cup, even in the presence of acetabular bone defects.

Original languageEnglish
Pages (from-to)665-670
Number of pages6
JournalJournal of Orthopaedic Science
Volume23
Issue number4
DOIs
Publication statusPublished - Jul 2018

Fingerprint

Titanium
Bone and Bones
Torque
Porosity

All Science Journal Classification (ASJC) codes

  • Surgery
  • Orthopedics and Sports Medicine

Cite this

Initial stability of a highly porous titanium cup in an acetabular bone defect model. / Yoshimoto, Kensei; Nakashima, Yasuharu; Wakiyama, Miyo; Hara, Daisuke; Nakamura, Akihiro; Iwamoto, Mikio.

In: Journal of Orthopaedic Science, Vol. 23, No. 4, 07.2018, p. 665-670.

Research output: Contribution to journalArticle

Yoshimoto, Kensei ; Nakashima, Yasuharu ; Wakiyama, Miyo ; Hara, Daisuke ; Nakamura, Akihiro ; Iwamoto, Mikio. / Initial stability of a highly porous titanium cup in an acetabular bone defect model. In: Journal of Orthopaedic Science. 2018 ; Vol. 23, No. 4. pp. 665-670.
@article{968ba2d03cbe485f89e57184e5c9db7e,
title = "Initial stability of a highly porous titanium cup in an acetabular bone defect model",
abstract = "Backgrounds: The purpose of this study was to quantify the initial stability of a highly porous titanium cup using an acetabular bone defect model. Methods: The maximum torque of a highly porous titanium cup, with a pore size of 640 μm and porosity of 60{\%}, was measured using rotational and lever-out torque testing and compared to that of a titanium-sprayed cup. The bone models were prepared using a polyurethane foam block and had three levels of bone coverage: 100, 70, and 50{\%}. Results: The highly porous titanium cup demonstrated significantly higher maximum torque than the titanium-sprayed cups in the three levels of bone defects. On rotational torque testing, it was found to be 1.5, 1.3, and 1.3 times stronger than the titanium-sprayed cups with 100, 70 and 50{\%} bone coverage, respectively. Furthermore, it was found to be 2.2, 2.3, and 1.5 times stronger on lever-out testing than the titanium-sprayed cup. No breakage in the porous layers was noted during the testing. Conclusion: This study provides additional evidence of the initial stability of highly porous titanium cup, even in the presence of acetabular bone defects.",
author = "Kensei Yoshimoto and Yasuharu Nakashima and Miyo Wakiyama and Daisuke Hara and Akihiro Nakamura and Mikio Iwamoto",
year = "2018",
month = "7",
doi = "10.1016/j.jos.2018.03.007",
language = "English",
volume = "23",
pages = "665--670",
journal = "Journal of Orthopaedic Science",
issn = "0949-2658",
publisher = "Springer Japan",
number = "4",

}

TY - JOUR

T1 - Initial stability of a highly porous titanium cup in an acetabular bone defect model

AU - Yoshimoto, Kensei

AU - Nakashima, Yasuharu

AU - Wakiyama, Miyo

AU - Hara, Daisuke

AU - Nakamura, Akihiro

AU - Iwamoto, Mikio

PY - 2018/7

Y1 - 2018/7

N2 - Backgrounds: The purpose of this study was to quantify the initial stability of a highly porous titanium cup using an acetabular bone defect model. Methods: The maximum torque of a highly porous titanium cup, with a pore size of 640 μm and porosity of 60%, was measured using rotational and lever-out torque testing and compared to that of a titanium-sprayed cup. The bone models were prepared using a polyurethane foam block and had three levels of bone coverage: 100, 70, and 50%. Results: The highly porous titanium cup demonstrated significantly higher maximum torque than the titanium-sprayed cups in the three levels of bone defects. On rotational torque testing, it was found to be 1.5, 1.3, and 1.3 times stronger than the titanium-sprayed cups with 100, 70 and 50% bone coverage, respectively. Furthermore, it was found to be 2.2, 2.3, and 1.5 times stronger on lever-out testing than the titanium-sprayed cup. No breakage in the porous layers was noted during the testing. Conclusion: This study provides additional evidence of the initial stability of highly porous titanium cup, even in the presence of acetabular bone defects.

AB - Backgrounds: The purpose of this study was to quantify the initial stability of a highly porous titanium cup using an acetabular bone defect model. Methods: The maximum torque of a highly porous titanium cup, with a pore size of 640 μm and porosity of 60%, was measured using rotational and lever-out torque testing and compared to that of a titanium-sprayed cup. The bone models were prepared using a polyurethane foam block and had three levels of bone coverage: 100, 70, and 50%. Results: The highly porous titanium cup demonstrated significantly higher maximum torque than the titanium-sprayed cups in the three levels of bone defects. On rotational torque testing, it was found to be 1.5, 1.3, and 1.3 times stronger than the titanium-sprayed cups with 100, 70 and 50% bone coverage, respectively. Furthermore, it was found to be 2.2, 2.3, and 1.5 times stronger on lever-out testing than the titanium-sprayed cup. No breakage in the porous layers was noted during the testing. Conclusion: This study provides additional evidence of the initial stability of highly porous titanium cup, even in the presence of acetabular bone defects.

UR - http://www.scopus.com/inward/record.url?scp=85045239529&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=85045239529&partnerID=8YFLogxK

U2 - 10.1016/j.jos.2018.03.007

DO - 10.1016/j.jos.2018.03.007

M3 - Article

C2 - 29657105

AN - SCOPUS:85045239529

VL - 23

SP - 665

EP - 670

JO - Journal of Orthopaedic Science

JF - Journal of Orthopaedic Science

SN - 0949-2658

IS - 4

ER -