Fingerprint
Dive into the research topics of 'Mechanical properties of injection molded superalloy (rene 95) compacts at high temperature'. Together they form a unique fingerprint.- Sort by
- Weight
- Alphabetically
Hideshi Miura, Toshiko Osada, Shunsuke Morinaka, Hyungoo Kang, Fujio Tsumori
Research output: Chapter in Book/Report/Conference proceeding › Conference contribution