Abstract
A mesophase pitch spinnable at moderate temperatures has been prepared by a two-stage heat-treatment process. The yield of mesophase pitch with 100 vol% anisotropy from coal-tar pitch was increased to 30-60 wt%.
Original language | English |
---|---|
Pages (from-to) | 355-358 |
Number of pages | 4 |
Journal | High Temperatures - High Pressures |
Volume | 22 |
Issue number | 3 |
Publication status | Published - 1990 |
Externally published | Yes |
Event | International Symposium on the Development of Carbon Fibres and Their Applications - Seoul, South Korea Duration: Mar 19 1990 → Mar 24 1990 |
All Science Journal Classification (ASJC) codes
- Condensed Matter Physics
- Mechanics of Materials
- Physical and Theoretical Chemistry