Sn concentration dependence of magnetic properties of Pr(Pb 1-xSnx)3

Kenji Yurue, Tatsuya Kawae, Masaki Mito, Masako Hitaka, Kazuyoshi Takeda, Hiroumi Ishii, Tetsuo Kitai

Research output: Contribution to journalArticle

Abstract

We have studied the low-temperature properties of Pr(Pb 1-xSnx)3 for a wide range of Sn concentration by measuring specific heat and susceptibility. In PrPb3 a sharp peak is observed at TQ = 0.4 K in the specific heat, which is due to a quadrupolar ordering. For x = 0.03, the peak is suppressed below 0.1 K, while the peak shifts to higher temperatures with further increase of Sn concentration. For x = 0.2, the peak is observed at ∼0.2 K. The possible origin of this behavior will be discussed.

Original languageEnglish
Pages (from-to)665-666
Number of pages2
JournalPhysica B: Condensed Matter
Volume329-333
Issue numberII
DOIs
Publication statusPublished - Jan 1 2003

Fingerprint

Specific heat
Magnetic properties
Low temperature properties
magnetic properties
specific heat
magnetic permeability
Temperature
shift

All Science Journal Classification (ASJC) codes

  • Electronic, Optical and Magnetic Materials
  • Condensed Matter Physics
  • Electrical and Electronic Engineering

Cite this

Sn concentration dependence of magnetic properties of Pr(Pb 1-xSnx)3 . / Yurue, Kenji; Kawae, Tatsuya; Mito, Masaki; Hitaka, Masako; Takeda, Kazuyoshi; Ishii, Hiroumi; Kitai, Tetsuo.

In: Physica B: Condensed Matter, Vol. 329-333, No. II, 01.01.2003, p. 665-666.

Research output: Contribution to journalArticle

Yurue, K, Kawae, T, Mito, M, Hitaka, M, Takeda, K, Ishii, H & Kitai, T 2003, 'Sn concentration dependence of magnetic properties of Pr(Pb 1-xSnx)3 ', Physica B: Condensed Matter, vol. 329-333, no. II, pp. 665-666. https://doi.org/10.1016/S0921-4526(02)02515-2
Yurue, Kenji ; Kawae, Tatsuya ; Mito, Masaki ; Hitaka, Masako ; Takeda, Kazuyoshi ; Ishii, Hiroumi ; Kitai, Tetsuo. / Sn concentration dependence of magnetic properties of Pr(Pb 1-xSnx)3 In: Physica B: Condensed Matter. 2003 ; Vol. 329-333, No. II. pp. 665-666.
@article{3f4cb12e69e543699cc487c76c411f8b,
title = "Sn concentration dependence of magnetic properties of Pr(Pb 1-xSnx)3",
abstract = "We have studied the low-temperature properties of Pr(Pb 1-xSnx)3 for a wide range of Sn concentration by measuring specific heat and susceptibility. In PrPb3 a sharp peak is observed at TQ = 0.4 K in the specific heat, which is due to a quadrupolar ordering. For x = 0.03, the peak is suppressed below 0.1 K, while the peak shifts to higher temperatures with further increase of Sn concentration. For x = 0.2, the peak is observed at ∼0.2 K. The possible origin of this behavior will be discussed.",
author = "Kenji Yurue and Tatsuya Kawae and Masaki Mito and Masako Hitaka and Kazuyoshi Takeda and Hiroumi Ishii and Tetsuo Kitai",
year = "2003",
month = "1",
day = "1",
doi = "10.1016/S0921-4526(02)02515-2",
language = "English",
volume = "329-333",
pages = "665--666",
journal = "Physica B: Condensed Matter",
issn = "0921-4526",
publisher = "Elsevier",
number = "II",

}

TY - JOUR

T1 - Sn concentration dependence of magnetic properties of Pr(Pb 1-xSnx)3

AU - Yurue, Kenji

AU - Kawae, Tatsuya

AU - Mito, Masaki

AU - Hitaka, Masako

AU - Takeda, Kazuyoshi

AU - Ishii, Hiroumi

AU - Kitai, Tetsuo

PY - 2003/1/1

Y1 - 2003/1/1

N2 - We have studied the low-temperature properties of Pr(Pb 1-xSnx)3 for a wide range of Sn concentration by measuring specific heat and susceptibility. In PrPb3 a sharp peak is observed at TQ = 0.4 K in the specific heat, which is due to a quadrupolar ordering. For x = 0.03, the peak is suppressed below 0.1 K, while the peak shifts to higher temperatures with further increase of Sn concentration. For x = 0.2, the peak is observed at ∼0.2 K. The possible origin of this behavior will be discussed.

AB - We have studied the low-temperature properties of Pr(Pb 1-xSnx)3 for a wide range of Sn concentration by measuring specific heat and susceptibility. In PrPb3 a sharp peak is observed at TQ = 0.4 K in the specific heat, which is due to a quadrupolar ordering. For x = 0.03, the peak is suppressed below 0.1 K, while the peak shifts to higher temperatures with further increase of Sn concentration. For x = 0.2, the peak is observed at ∼0.2 K. The possible origin of this behavior will be discussed.

UR - http://www.scopus.com/inward/record.url?scp=23044490773&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=23044490773&partnerID=8YFLogxK

U2 - 10.1016/S0921-4526(02)02515-2

DO - 10.1016/S0921-4526(02)02515-2

M3 - Article

AN - SCOPUS:23044490773

VL - 329-333

SP - 665

EP - 666

JO - Physica B: Condensed Matter

JF - Physica B: Condensed Matter

SN - 0921-4526

IS - II

ER -