Biopex® acquires anti-washout properties by adding sodium alginate into its liquid phase

Satoru Tanaka, Tamisuke Kishi, Ryoji Shimogoryo, Shigeki Matsuya, Kunio Ishikawa

研究成果: Contribution to journalArticle査読

28 被引用数 (Scopus)

抄録

Biopex® sets upon mixing with its liquid phase due to chelate reaction between sodium succinate and calcium phosphate, then gradually transforms to apatite. As a result of apatite formation, set Biopex® shows excellent tissue responses and good osteoconductivity. However, Biopex would be washed out when the paste is exposed to body fluid before its setting reaction. Washed out cement causes an inflammatory response. In this investigation, therefore, sodium alginate was added to the liquid phase of Biopex® and its effects on washout properties and transformation to apatite were studied. We found that cement remaining ratio, an index of the anti-washout property, of the Biopex® increased by increasing the amounts of added sodium alginate to reach 100% when the liquid phase of Biopex® contained 0.6% or more sodium alginate. Biopex® gradually transformed to apatite regardless of the amount of added sodium alginate at least when the concentration of the sodium alginate in the liquid phase was 1.0% or less. It is concluded therefore, that addition of sodium alginate is very useful for Biopex® to acquire the anti-washout property.

本文言語英語
ページ(範囲)301-312
ページ数12
ジャーナルdental materials journal
22
3
DOI
出版ステータス出版済み - 9 2003

All Science Journal Classification (ASJC) codes

  • Ceramics and Composites
  • Dentistry(all)

フィンガープリント 「Biopex® acquires anti-washout properties by adding sodium alginate into its liquid phase」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。