We investigated the mechanical properties of B2-type FeCo based alloys containing minor amounts of Ni or Pd to improve their tensile ductility at room temperature. The yield and tensile stresses of the new alloys showed remarkable increases. FeCoNi alloys showed high total elongation of over 10% at room temperature. Co50Fe40Pd10 alloy displayed a tensile strength of 1250MPa and a high total elongation of 16%. The substitution of Ni or Pd into FeCo based alloys is therefore an extremely effective means of improving their room-temperature ductility.

元の言語英語
ページ(範囲)1826-1828
ページ数3
ジャーナルMaterials Transactions
53
発行部数10
DOI
出版物ステータス出版済み - 10 5 2012

Fingerprint

ductility
elongation
Ductility
Elongation
room temperature
tensile stress
Tensile stress
Temperature
tensile strength
Yield stress
Substitution reactions
Tensile strength
mechanical properties
substitutes
Mechanical properties

All Science Journal Classification (ASJC) codes

  • Materials Science(all)
  • Condensed Matter Physics
  • Mechanical Engineering
  • Mechanics of Materials

これを引用

Matsuda, M., Yamashita, K., Sago, R., Akamine, K., Takashima, K., & Nishida, M. (2012). Development of ductile B2-Type Fe-Co based alloys. Materials Transactions, 53(10), 1826-1828. https://doi.org/10.2320/matertrans.M2012205

Development of ductile B2-Type Fe-Co based alloys. / Matsuda, Mitsuhiro; Yamashita, Kozo; Sago, Ryutaro; Akamine, Kenji; Takashima, Kazuki; Nishida, Minoru.

:: Materials Transactions, 巻 53, 番号 10, 05.10.2012, p. 1826-1828.

研究成果: ジャーナルへの寄稿記事

Matsuda, M, Yamashita, K, Sago, R, Akamine, K, Takashima, K & Nishida, M 2012, 'Development of ductile B2-Type Fe-Co based alloys', Materials Transactions, 巻. 53, 番号 10, pp. 1826-1828. https://doi.org/10.2320/matertrans.M2012205
Matsuda M, Yamashita K, Sago R, Akamine K, Takashima K, Nishida M. Development of ductile B2-Type Fe-Co based alloys. Materials Transactions. 2012 10 5;53(10):1826-1828. https://doi.org/10.2320/matertrans.M2012205
Matsuda, Mitsuhiro ; Yamashita, Kozo ; Sago, Ryutaro ; Akamine, Kenji ; Takashima, Kazuki ; Nishida, Minoru. / Development of ductile B2-Type Fe-Co based alloys. :: Materials Transactions. 2012 ; 巻 53, 番号 10. pp. 1826-1828.
@article{fe95a3892e5344a6a9cf008a9849f8cb,
title = "Development of ductile B2-Type Fe-Co based alloys",
abstract = "We investigated the mechanical properties of B2-type FeCo based alloys containing minor amounts of Ni or Pd to improve their tensile ductility at room temperature. The yield and tensile stresses of the new alloys showed remarkable increases. FeCoNi alloys showed high total elongation of over 10{\%} at room temperature. Co50Fe40Pd10 alloy displayed a tensile strength of 1250MPa and a high total elongation of 16{\%}. The substitution of Ni or Pd into FeCo based alloys is therefore an extremely effective means of improving their room-temperature ductility.",
author = "Mitsuhiro Matsuda and Kozo Yamashita and Ryutaro Sago and Kenji Akamine and Kazuki Takashima and Minoru Nishida",
year = "2012",
month = "10",
day = "5",
doi = "10.2320/matertrans.M2012205",
language = "English",
volume = "53",
pages = "1826--1828",
journal = "Materials Transactions",
issn = "0916-1821",
publisher = "The Japan Institute of Metals and Materials",
number = "10",

}

TY - JOUR

T1 - Development of ductile B2-Type Fe-Co based alloys

AU - Matsuda, Mitsuhiro

AU - Yamashita, Kozo

AU - Sago, Ryutaro

AU - Akamine, Kenji

AU - Takashima, Kazuki

AU - Nishida, Minoru

PY - 2012/10/5

Y1 - 2012/10/5

N2 - We investigated the mechanical properties of B2-type FeCo based alloys containing minor amounts of Ni or Pd to improve their tensile ductility at room temperature. The yield and tensile stresses of the new alloys showed remarkable increases. FeCoNi alloys showed high total elongation of over 10% at room temperature. Co50Fe40Pd10 alloy displayed a tensile strength of 1250MPa and a high total elongation of 16%. The substitution of Ni or Pd into FeCo based alloys is therefore an extremely effective means of improving their room-temperature ductility.

AB - We investigated the mechanical properties of B2-type FeCo based alloys containing minor amounts of Ni or Pd to improve their tensile ductility at room temperature. The yield and tensile stresses of the new alloys showed remarkable increases. FeCoNi alloys showed high total elongation of over 10% at room temperature. Co50Fe40Pd10 alloy displayed a tensile strength of 1250MPa and a high total elongation of 16%. The substitution of Ni or Pd into FeCo based alloys is therefore an extremely effective means of improving their room-temperature ductility.

UR - http://www.scopus.com/inward/record.url?scp=84866896660&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84866896660&partnerID=8YFLogxK

U2 - 10.2320/matertrans.M2012205

DO - 10.2320/matertrans.M2012205

M3 - Article

AN - SCOPUS:84866896660

VL - 53

SP - 1826

EP - 1828

JO - Materials Transactions

JF - Materials Transactions

SN - 0916-1821

IS - 10

ER -