JFE Group has produced phthalic anhydride at its Chiba plant since 1979 by using a fluidized bed reactor. A ground silica-based catalyst was used at the beginning of fluidized bed operation. By changing to a spherical type catalyst, the duration of catalytic activity was increased and catalyst density in the bed was reduced by around 10%. Addition of Cs to the catalyst enhanced its activity. Non-active silica gel was used as diluent for matching catalyst activity with plant capacity. The active component of Cs added to the catalyst has a lower melting point, the catalyst particles bound with it. The fluidized bed was operated stably by controlling the Cs/K ratio.

元の言語英語
ページ(範囲)272-276
ページ数5
ジャーナルkagaku kogaku ronbunshu
30
発行部数3
DOI
出版物ステータス出版済み - 5 1 2004

Fingerprint

Fluidized beds
Catalysts
Catalyst activity
Silica Gel
Silica gel
Silicon Dioxide
Melting point
phthalic anhydride
Silica

All Science Journal Classification (ASJC) codes

  • Chemistry(all)
  • Chemical Engineering(all)

これを引用

Development of fluidized bed catalyst for phthalic anhydride production. / Saima, Hitoshi; Aono, Toshinao; Asami, Yukio; Nobusawa, Tatsuya; Suzuki, Toshihide.

:: kagaku kogaku ronbunshu, 巻 30, 番号 3, 01.05.2004, p. 272-276.

研究成果: ジャーナルへの寄稿記事

Saima, Hitoshi ; Aono, Toshinao ; Asami, Yukio ; Nobusawa, Tatsuya ; Suzuki, Toshihide. / Development of fluidized bed catalyst for phthalic anhydride production. :: kagaku kogaku ronbunshu. 2004 ; 巻 30, 番号 3. pp. 272-276.
@article{645346b92ad4482a8ff956f8c69188c9,
title = "Development of fluidized bed catalyst for phthalic anhydride production",
abstract = "JFE Group has produced phthalic anhydride at its Chiba plant since 1979 by using a fluidized bed reactor. A ground silica-based catalyst was used at the beginning of fluidized bed operation. By changing to a spherical type catalyst, the duration of catalytic activity was increased and catalyst density in the bed was reduced by around 10{\%}. Addition of Cs to the catalyst enhanced its activity. Non-active silica gel was used as diluent for matching catalyst activity with plant capacity. The active component of Cs added to the catalyst has a lower melting point, the catalyst particles bound with it. The fluidized bed was operated stably by controlling the Cs/K ratio.",
author = "Hitoshi Saima and Toshinao Aono and Yukio Asami and Tatsuya Nobusawa and Toshihide Suzuki",
year = "2004",
month = "5",
day = "1",
doi = "10.1252/kakoronbunshu.30.272",
language = "English",
volume = "30",
pages = "272--276",
journal = "Kagaku Kogaku Ronbunshu",
issn = "0386-216X",
publisher = "The Society of Chemical Engineers, Japan",
number = "3",

}

TY - JOUR

T1 - Development of fluidized bed catalyst for phthalic anhydride production

AU - Saima, Hitoshi

AU - Aono, Toshinao

AU - Asami, Yukio

AU - Nobusawa, Tatsuya

AU - Suzuki, Toshihide

PY - 2004/5/1

Y1 - 2004/5/1

N2 - JFE Group has produced phthalic anhydride at its Chiba plant since 1979 by using a fluidized bed reactor. A ground silica-based catalyst was used at the beginning of fluidized bed operation. By changing to a spherical type catalyst, the duration of catalytic activity was increased and catalyst density in the bed was reduced by around 10%. Addition of Cs to the catalyst enhanced its activity. Non-active silica gel was used as diluent for matching catalyst activity with plant capacity. The active component of Cs added to the catalyst has a lower melting point, the catalyst particles bound with it. The fluidized bed was operated stably by controlling the Cs/K ratio.

AB - JFE Group has produced phthalic anhydride at its Chiba plant since 1979 by using a fluidized bed reactor. A ground silica-based catalyst was used at the beginning of fluidized bed operation. By changing to a spherical type catalyst, the duration of catalytic activity was increased and catalyst density in the bed was reduced by around 10%. Addition of Cs to the catalyst enhanced its activity. Non-active silica gel was used as diluent for matching catalyst activity with plant capacity. The active component of Cs added to the catalyst has a lower melting point, the catalyst particles bound with it. The fluidized bed was operated stably by controlling the Cs/K ratio.

UR - http://www.scopus.com/inward/record.url?scp=4344597307&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=4344597307&partnerID=8YFLogxK

U2 - 10.1252/kakoronbunshu.30.272

DO - 10.1252/kakoronbunshu.30.272

M3 - Article

AN - SCOPUS:4344597307

VL - 30

SP - 272

EP - 276

JO - Kagaku Kogaku Ronbunshu

JF - Kagaku Kogaku Ronbunshu

SN - 0386-216X

IS - 3

ER -