The effect of equal-channel angular pressing (ECAP) on the pitting corrosion of pure Al was investigated using electrochemical techniques in solutions containing 0.1 m mol·dm-3 of Na2SO 4 and 8.46 mol·dm-3 of NaCl (300 ppm Cl -) and followed by surface analysis. The potential for pitting corrosion of pure Al was clearly shifted in the noble direction by the ECAP process indicating that this process improves resistance to pitting corrosion. The time dependence of corrosion potential and the anodic potential at 1 A·m-2 revealed that the rate of formation of Al oxide films increased due to a decrease in the grain size of the Al after ECAP. Since there exists a negligible amount of impurity precipitates in pure Al, the improvement in pitting corrosion resistance of pure Al by ECAP appears to be attributable to an increase in the rate of formation of Al oxide films.

元の言語英語
記事番号450854
ジャーナルInternational Journal of Corrosion
2012
DOI
出版物ステータス出版済み - 12 1 2012
外部発表Yes

Fingerprint

Equal channel angular pressing
Pitting
Aluminum
Corrosion
Oxide films
Surface analysis
Corrosion resistance
Precipitates
Impurities

All Science Journal Classification (ASJC) codes

  • Materials Science(all)
  • Process Chemistry and Technology

これを引用

Effect of equal-channel angular pressing on pitting corrosion of pure aluminum. / Son, Injoon; Nakano, Hiroaki; Oue, Satoshi; Kobayashi, Shigeo; Fukushima, Hisaaki; Horita, Zenji.

:: International Journal of Corrosion, 巻 2012, 450854, 01.12.2012.

研究成果: ジャーナルへの寄稿記事

Son, Injoon ; Nakano, Hiroaki ; Oue, Satoshi ; Kobayashi, Shigeo ; Fukushima, Hisaaki ; Horita, Zenji. / Effect of equal-channel angular pressing on pitting corrosion of pure aluminum. :: International Journal of Corrosion. 2012 ; 巻 2012.
@article{79746214074c41d59ac988c7ba014722,
title = "Effect of equal-channel angular pressing on pitting corrosion of pure aluminum",
abstract = "The effect of equal-channel angular pressing (ECAP) on the pitting corrosion of pure Al was investigated using electrochemical techniques in solutions containing 0.1 m mol·dm-3 of Na2SO 4 and 8.46 mol·dm-3 of NaCl (300 ppm Cl -) and followed by surface analysis. The potential for pitting corrosion of pure Al was clearly shifted in the noble direction by the ECAP process indicating that this process improves resistance to pitting corrosion. The time dependence of corrosion potential and the anodic potential at 1 A·m-2 revealed that the rate of formation of Al oxide films increased due to a decrease in the grain size of the Al after ECAP. Since there exists a negligible amount of impurity precipitates in pure Al, the improvement in pitting corrosion resistance of pure Al by ECAP appears to be attributable to an increase in the rate of formation of Al oxide films.",
author = "Injoon Son and Hiroaki Nakano and Satoshi Oue and Shigeo Kobayashi and Hisaaki Fukushima and Zenji Horita",
year = "2012",
month = "12",
day = "1",
doi = "10.1155/2012/450854",
language = "English",
volume = "2012",
journal = "International Journal of Corrosion",
issn = "1687-9325",
publisher = "Hindawi Publishing Corporation",

}

TY - JOUR

T1 - Effect of equal-channel angular pressing on pitting corrosion of pure aluminum

AU - Son, Injoon

AU - Nakano, Hiroaki

AU - Oue, Satoshi

AU - Kobayashi, Shigeo

AU - Fukushima, Hisaaki

AU - Horita, Zenji

PY - 2012/12/1

Y1 - 2012/12/1

N2 - The effect of equal-channel angular pressing (ECAP) on the pitting corrosion of pure Al was investigated using electrochemical techniques in solutions containing 0.1 m mol·dm-3 of Na2SO 4 and 8.46 mol·dm-3 of NaCl (300 ppm Cl -) and followed by surface analysis. The potential for pitting corrosion of pure Al was clearly shifted in the noble direction by the ECAP process indicating that this process improves resistance to pitting corrosion. The time dependence of corrosion potential and the anodic potential at 1 A·m-2 revealed that the rate of formation of Al oxide films increased due to a decrease in the grain size of the Al after ECAP. Since there exists a negligible amount of impurity precipitates in pure Al, the improvement in pitting corrosion resistance of pure Al by ECAP appears to be attributable to an increase in the rate of formation of Al oxide films.

AB - The effect of equal-channel angular pressing (ECAP) on the pitting corrosion of pure Al was investigated using electrochemical techniques in solutions containing 0.1 m mol·dm-3 of Na2SO 4 and 8.46 mol·dm-3 of NaCl (300 ppm Cl -) and followed by surface analysis. The potential for pitting corrosion of pure Al was clearly shifted in the noble direction by the ECAP process indicating that this process improves resistance to pitting corrosion. The time dependence of corrosion potential and the anodic potential at 1 A·m-2 revealed that the rate of formation of Al oxide films increased due to a decrease in the grain size of the Al after ECAP. Since there exists a negligible amount of impurity precipitates in pure Al, the improvement in pitting corrosion resistance of pure Al by ECAP appears to be attributable to an increase in the rate of formation of Al oxide films.

UR - http://www.scopus.com/inward/record.url?scp=84873875673&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84873875673&partnerID=8YFLogxK

U2 - 10.1155/2012/450854

DO - 10.1155/2012/450854

M3 - Article

VL - 2012

JO - International Journal of Corrosion

JF - International Journal of Corrosion

SN - 1687-9325

M1 - 450854

ER -