Effect of tensile strain rate on ductile fracture energy for industrial pure iron

Takuya Nishimura, Masatoshi Aramaki, Shinji Munetoh, Rintaro Ueji, Osamu Furukimi

研究成果: 著書/レポートタイプへの貢献会議での発言

抄録

The effect of tensile strain rate on the formation of voids by using the industrial pure iron (0.0028% C,-0.16% Mn,-0.001% Si) with few precipitates was studied. The tensile tests were performed under the initial strain rate of 10-3,101 and 103 s-1. The void distribution, the void spacing and the deformation energy in each strain rate were examined. From these experiments, it was revealed that the energy required for the coalescence of voids was increased with the increase in void spacing and the suppression of void generation by increasing the strain rate improved the local deformation energy.

元の言語英語
ホスト出版物のタイトルProceedings - European Conference on Heat Treatment and 21st IFHTSE Congress
編集者Thomas Lubben, Hans-Werner Zoch, Reinhold Schneider
出版者Arbeitsgemeineschaft Warmebehandlung u. Werkstofftechnik
ページ511-514
ページ数4
ISBN(電子版)9780000000002
出版物ステータス出版済み - 1 1 2014
イベントEuropean Conference on Heat Treatment and 21st IFHTSE Congress - Munich, ドイツ
継続期間: 5 12 20145 15 2014

出版物シリーズ

名前Proceedings - European Conference on Heat Treatment and 21st IFHTSE Congress

その他

その他European Conference on Heat Treatment and 21st IFHTSE Congress
ドイツ
Munich
期間5/12/145/15/14

Fingerprint

Fracture energy
Ductile fracture
Tensile strain
Strain rate
Iron
Coalescence
Precipitates
Experiments

All Science Journal Classification (ASJC) codes

  • Energy Engineering and Power Technology
  • Materials Science(all)
  • Fluid Flow and Transfer Processes

これを引用

Nishimura, T., Aramaki, M., Munetoh, S., Ueji, R., & Furukimi, O. (2014). Effect of tensile strain rate on ductile fracture energy for industrial pure iron. : T. Lubben, H-W. Zoch, & R. Schneider (版), Proceedings - European Conference on Heat Treatment and 21st IFHTSE Congress (pp. 511-514). (Proceedings - European Conference on Heat Treatment and 21st IFHTSE Congress). Arbeitsgemeineschaft Warmebehandlung u. Werkstofftechnik.

Effect of tensile strain rate on ductile fracture energy for industrial pure iron. / Nishimura, Takuya; Aramaki, Masatoshi; Munetoh, Shinji; Ueji, Rintaro; Furukimi, Osamu.

Proceedings - European Conference on Heat Treatment and 21st IFHTSE Congress. 版 / Thomas Lubben; Hans-Werner Zoch; Reinhold Schneider. Arbeitsgemeineschaft Warmebehandlung u. Werkstofftechnik, 2014. p. 511-514 (Proceedings - European Conference on Heat Treatment and 21st IFHTSE Congress).

研究成果: 著書/レポートタイプへの貢献会議での発言

Nishimura, T, Aramaki, M, Munetoh, S, Ueji, R & Furukimi, O 2014, Effect of tensile strain rate on ductile fracture energy for industrial pure iron. : T Lubben, H-W Zoch & R Schneider (版), Proceedings - European Conference on Heat Treatment and 21st IFHTSE Congress. Proceedings - European Conference on Heat Treatment and 21st IFHTSE Congress, Arbeitsgemeineschaft Warmebehandlung u. Werkstofftechnik, pp. 511-514, European Conference on Heat Treatment and 21st IFHTSE Congress, Munich, ドイツ, 5/12/14.
Nishimura T, Aramaki M, Munetoh S, Ueji R, Furukimi O. Effect of tensile strain rate on ductile fracture energy for industrial pure iron. : Lubben T, Zoch H-W, Schneider R, 編集者, Proceedings - European Conference on Heat Treatment and 21st IFHTSE Congress. Arbeitsgemeineschaft Warmebehandlung u. Werkstofftechnik. 2014. p. 511-514. (Proceedings - European Conference on Heat Treatment and 21st IFHTSE Congress).
Nishimura, Takuya ; Aramaki, Masatoshi ; Munetoh, Shinji ; Ueji, Rintaro ; Furukimi, Osamu. / Effect of tensile strain rate on ductile fracture energy for industrial pure iron. Proceedings - European Conference on Heat Treatment and 21st IFHTSE Congress. 編集者 / Thomas Lubben ; Hans-Werner Zoch ; Reinhold Schneider. Arbeitsgemeineschaft Warmebehandlung u. Werkstofftechnik, 2014. pp. 511-514 (Proceedings - European Conference on Heat Treatment and 21st IFHTSE Congress).
@inproceedings{bd3b136cd00b4dae89f5fca03bb6ece3,
title = "Effect of tensile strain rate on ductile fracture energy for industrial pure iron",
abstract = "The effect of tensile strain rate on the formation of voids by using the industrial pure iron (0.0028{\%} C,-0.16{\%} Mn,-0.001{\%} Si) with few precipitates was studied. The tensile tests were performed under the initial strain rate of 10-3,101 and 103 s-1. The void distribution, the void spacing and the deformation energy in each strain rate were examined. From these experiments, it was revealed that the energy required for the coalescence of voids was increased with the increase in void spacing and the suppression of void generation by increasing the strain rate improved the local deformation energy.",
author = "Takuya Nishimura and Masatoshi Aramaki and Shinji Munetoh and Rintaro Ueji and Osamu Furukimi",
year = "2014",
month = "1",
day = "1",
language = "English",
series = "Proceedings - European Conference on Heat Treatment and 21st IFHTSE Congress",
publisher = "Arbeitsgemeineschaft Warmebehandlung u. Werkstofftechnik",
pages = "511--514",
editor = "Thomas Lubben and Hans-Werner Zoch and Reinhold Schneider",
booktitle = "Proceedings - European Conference on Heat Treatment and 21st IFHTSE Congress",

}

TY - GEN

T1 - Effect of tensile strain rate on ductile fracture energy for industrial pure iron

AU - Nishimura, Takuya

AU - Aramaki, Masatoshi

AU - Munetoh, Shinji

AU - Ueji, Rintaro

AU - Furukimi, Osamu

PY - 2014/1/1

Y1 - 2014/1/1

N2 - The effect of tensile strain rate on the formation of voids by using the industrial pure iron (0.0028% C,-0.16% Mn,-0.001% Si) with few precipitates was studied. The tensile tests were performed under the initial strain rate of 10-3,101 and 103 s-1. The void distribution, the void spacing and the deformation energy in each strain rate were examined. From these experiments, it was revealed that the energy required for the coalescence of voids was increased with the increase in void spacing and the suppression of void generation by increasing the strain rate improved the local deformation energy.

AB - The effect of tensile strain rate on the formation of voids by using the industrial pure iron (0.0028% C,-0.16% Mn,-0.001% Si) with few precipitates was studied. The tensile tests were performed under the initial strain rate of 10-3,101 and 103 s-1. The void distribution, the void spacing and the deformation energy in each strain rate were examined. From these experiments, it was revealed that the energy required for the coalescence of voids was increased with the increase in void spacing and the suppression of void generation by increasing the strain rate improved the local deformation energy.

UR - http://www.scopus.com/inward/record.url?scp=84915798862&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84915798862&partnerID=8YFLogxK

M3 - Conference contribution

AN - SCOPUS:84915798862

T3 - Proceedings - European Conference on Heat Treatment and 21st IFHTSE Congress

SP - 511

EP - 514

BT - Proceedings - European Conference on Heat Treatment and 21st IFHTSE Congress

A2 - Lubben, Thomas

A2 - Zoch, Hans-Werner

A2 - Schneider, Reinhold

PB - Arbeitsgemeineschaft Warmebehandlung u. Werkstofftechnik

ER -