抄録
Polyvinyl chloride pitch was blended with coal-tar-based mesophase pitch with the aim of improving the stabilization reactivity of the pitch fibres. They were found to be highly compatible and reduced the oxidative stabilization time for the fibres to maintain their form during carbonization at over 600 degrees C from 120 to 80 min.
本文言語 | 英語 |
---|---|
ジャーナル | [No source information available] |
出版ステータス | 出版済み - 1月 1 1987 |
!!!All Science Journal Classification (ASJC) codes
- 材料科学(全般)