N2 - Rotating bending fatigue tests were carried out for Inconel 718 at room temperature and elevated temperatures of 300 °C, 500 °C and 600 °C to investigate the influence of temperature on the fatigue crack growth resistance. The crack growth rate can be expressed by the small crack growth law, dl/dN = C1σanl = C2(σa/σB)nl, at all the temperatures, where σB, σa and l are the tensile strength, the stress amplitude and the crack length, and C1, C2 and n are constants. Therefore, the resistance to crack growth was evaluated using the small crack growth law. The fatigue crack growth resistance decreased with the increase of temperature.
AB - Rotating bending fatigue tests were carried out for Inconel 718 at room temperature and elevated temperatures of 300 °C, 500 °C and 600 °C to investigate the influence of temperature on the fatigue crack growth resistance. The crack growth rate can be expressed by the small crack growth law, dl/dN = C1σanl = C2(σa/σB)nl, at all the temperatures, where σB, σa and l are the tensile strength, the stress amplitude and the crack length, and C1, C2 and n are constants. Therefore, the resistance to crack growth was evaluated using the small crack growth law. The fatigue crack growth resistance decreased with the increase of temperature.
UR - http://www.scopus.com/inward/record.url?scp=0031274959&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=0031274959&partnerID=8YFLogxK
U2 - 10.1299/kikaia.63.2298
DO - 10.1299/kikaia.63.2298
M3 - Article
AN - SCOPUS:0031274959
VL - 63
SP - 2298
EP - 2302
JO - Nihon Kikai Gakkai Ronbunshu, A Hen/Transactions of the Japan Society of Mechanical Engineers, Part A
JF - Nihon Kikai Gakkai Ronbunshu, A Hen/Transactions of the Japan Society of Mechanical Engineers, Part A
SN - 0387-5008
IS - 615
ER -