Fatigue crack initiation from small defects under low stress ratios in SAE52100 bearing steel

Y. Hino, H. Matsunaga

研究成果: 書籍/レポート タイプへの寄稿会議への寄与

抄録

Axial-loading fatigue tests were carried out under low stress ratios, R = -∞ ∼ -5.33, by use of a cylindrical specimen of SAE52100 bearing steel having drill holes of 50 ∼ 200 μm in diameter. The maximum stresses, σmax = 0 ∼ 300 MPa were combined with the minimum stresses, σmin of -1600 or -1800 MPa. Even at σmax = 0, fatigue cracks were initiated at hole edges by cyclic compressive stress of σmin = -1800 MPa, and the cracks finally became non-propagating. When σmax was positive, fatigue cracks were initiated even at σmin = -1600 MPa and they also became non-propagating. The length of non-propagating cracks increased with an increase in σmax. Those phenomena were considered to be related to the tensile residual stress that was induced by the plastic deformation in the vicinity of hole edges. The relationship between the length of non-propagating crack and the residual stress field was investigated in terms of elastic-plastic finite element analysis.

本文言語英語
ホスト出版物のタイトルFourth International Conference on Experimental Mechanics
DOI
出版ステータス出版済み - 12月 1 2010
外部発表はい
イベント4th International Conference on Experimental Mechanics - Singapore, シンガポール
継続期間: 11月 18 200911月 20 2009

出版物シリーズ

名前Proceedings of SPIE - The International Society for Optical Engineering
7522
ISSN(印刷版)0277-786X

その他

その他4th International Conference on Experimental Mechanics
国/地域シンガポール
CitySingapore
Period11/18/0911/20/09

!!!All Science Journal Classification (ASJC) codes

  • 電子材料、光学材料、および磁性材料
  • 凝縮系物理学
  • コンピュータ サイエンスの応用
  • 応用数学
  • 電子工学および電気工学

フィンガープリント

「Fatigue crack initiation from small defects under low stress ratios in SAE52100 bearing steel」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。

引用スタイル