TY - JOUR
T1 - Growth of Na2Ti6O13 whiskers from the high-temperature solutions of NaCl-TiO2 system
AU - Teshima, Katsuya
AU - Sugiura, Shiori
AU - Yubuta, Kunio
AU - Suzuki, Takaomi
AU - Endo, Morinobu
AU - Shishido, Toetsu
AU - Oishi, Shuji
PY - 2007/3
Y1 - 2007/3
N2 - The slow cooling of NaCl-TiO2 mixtures easily grew colorless and transparent Na2Ti6O13 whiskers. The whisker growth was conducted by heating a mixture of TiO2 and NaCl at 1100°C for 10 h, followed by cooling to 500°C at a rate of 5°C·h-1. Whiskers having average sizes of approximately 450 × 10 μm were grown from high-temperature solutions containing Ti of 0.3-13 mol%. The whiskers, which were hexagonal prisms, elongated in the 〈010〉 directions.
AB - The slow cooling of NaCl-TiO2 mixtures easily grew colorless and transparent Na2Ti6O13 whiskers. The whisker growth was conducted by heating a mixture of TiO2 and NaCl at 1100°C for 10 h, followed by cooling to 500°C at a rate of 5°C·h-1. Whiskers having average sizes of approximately 450 × 10 μm were grown from high-temperature solutions containing Ti of 0.3-13 mol%. The whiskers, which were hexagonal prisms, elongated in the 〈010〉 directions.
UR - http://www.scopus.com/inward/record.url?scp=33847732651&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=33847732651&partnerID=8YFLogxK
U2 - 10.2109/jcersj.115.230
DO - 10.2109/jcersj.115.230
M3 - Article
AN - SCOPUS:33847732651
VL - 115
SP - 230
EP - 232
JO - Nippon Seramikkusu Kyokai Gakujutsu Ronbunshi/Journal of the Ceramic Society of Japan
JF - Nippon Seramikkusu Kyokai Gakujutsu Ronbunshi/Journal of the Ceramic Society of Japan
SN - 1882-0743
IS - 1339
ER -