TY - JOUR
T1 - Hydrothermal synthesis of rutile crystalline by self-hydrolysis of TiOCl2
AU - Inada, Miki
AU - Mizue, Kei
AU - Hojo, Junichi
PY - 2008/4
Y1 - 2008/4
N2 - Rutile TiO2 nanoparticles were synthesized by self-hydrolysis of TiOCl2. Rutile phase was detected by XRD at 50°C. As the reacting temperature became higher, the XRD peaks of anatase appeared and the peak intensity of both phases became larger. The roundish agglomerates surrounded by acicular particles were observed by SEM at 50°C and acicular particles grew with elevating temperature. These results indicate that the crystal growth of rutile was promoted at high temperatures. When the pH value of starting solution became lower by addition of HCl, only rutile phase was detected by XRD even at high temperatures. This is because the deprotonation was suppressed under low pH value, leading to predominant formation of rutile. In this study, we obtained small acicular particles of rutile crystalline by addition of HNO3.
AB - Rutile TiO2 nanoparticles were synthesized by self-hydrolysis of TiOCl2. Rutile phase was detected by XRD at 50°C. As the reacting temperature became higher, the XRD peaks of anatase appeared and the peak intensity of both phases became larger. The roundish agglomerates surrounded by acicular particles were observed by SEM at 50°C and acicular particles grew with elevating temperature. These results indicate that the crystal growth of rutile was promoted at high temperatures. When the pH value of starting solution became lower by addition of HCl, only rutile phase was detected by XRD even at high temperatures. This is because the deprotonation was suppressed under low pH value, leading to predominant formation of rutile. In this study, we obtained small acicular particles of rutile crystalline by addition of HNO3.
UR - http://www.scopus.com/inward/record.url?scp=48249098489&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=48249098489&partnerID=8YFLogxK
U2 - 10.2497/jjspm.55.259
DO - 10.2497/jjspm.55.259
M3 - Article
AN - SCOPUS:48249098489
SN - 0532-8799
VL - 55
SP - 259
EP - 262
JO - Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy
JF - Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy
IS - 4
ER -