TY - JOUR
T1 - Maximum energy product of exchange-coupled Sm(FeCo)12/α-Fe nanocomposite particle
AU - Uda, Ryusei
AU - Koike, Kunihiro
AU - Inaba, Nobuyuki
AU - Kato, Hiroaki
AU - Itakura, Masaru
AU - Okubo, Susumu
AU - Ohta, Hitoshi
AU - Tsuchiura, Hiroki
N1 - Funding Information:
This work supported by JSPS KAKENHI Grant Numbers JP16H04488, JP20K05059 and JP20H02425 and the Joint Usage Research in Molecular Photoscience Research center in Kobe University, Japan (No. R04031).
Publisher Copyright:
© 2023 Author(s).
PY - 2023/2/1
Y1 - 2023/2/1
N2 - The effects of the coating surface orientation of the α-Fe soft magnetic layer on the Sm(Fe0.8Co0.2)12 hard magnetic phase and the volume fraction of α-Fe, VFe, on the maximum energy product, (BH)max of exchange-coupled Sm(Fe0.8Co0.2)12/α-Fe nanocomposite magnet particles were micromagnetics OOMMF package was systematically investigated. The (BH)max of the reference model, Sm(Fe0.8Co0.2)12 particles without Fe layer, was 630 kJ/m3. In contrast, in the nanocomposite magnet particle model with soft magnetic layers on both sides of the hard magnetic phase, (BH)max reached a maximum value of 657 kJ/m3 at VFe = 12% (Fe layer thickness, tFe = 2 nm). In the model with α-Fe coating on the top and bottom surfaces of the hard magnetic phase, (BH)max = 636 kJ/m3 at VFe = 4% (tFe = 2 nm). Furthermore, the coating of the soft magnetic phase on both sides of the hard phase particles reduces the magnitude of the demagnetizing field, Hd of the nanocomposite magnet particles, indicating that the side coating of the soft magnetic phase is effective in increasing (BH)max. These findings allow for a greater degree of freedom in the design of nanocomposite magnets by adjusting not only the VFe volume fraction of the hard/soft phases but also their arrangement.
AB - The effects of the coating surface orientation of the α-Fe soft magnetic layer on the Sm(Fe0.8Co0.2)12 hard magnetic phase and the volume fraction of α-Fe, VFe, on the maximum energy product, (BH)max of exchange-coupled Sm(Fe0.8Co0.2)12/α-Fe nanocomposite magnet particles were micromagnetics OOMMF package was systematically investigated. The (BH)max of the reference model, Sm(Fe0.8Co0.2)12 particles without Fe layer, was 630 kJ/m3. In contrast, in the nanocomposite magnet particle model with soft magnetic layers on both sides of the hard magnetic phase, (BH)max reached a maximum value of 657 kJ/m3 at VFe = 12% (Fe layer thickness, tFe = 2 nm). In the model with α-Fe coating on the top and bottom surfaces of the hard magnetic phase, (BH)max = 636 kJ/m3 at VFe = 4% (tFe = 2 nm). Furthermore, the coating of the soft magnetic phase on both sides of the hard phase particles reduces the magnitude of the demagnetizing field, Hd of the nanocomposite magnet particles, indicating that the side coating of the soft magnetic phase is effective in increasing (BH)max. These findings allow for a greater degree of freedom in the design of nanocomposite magnets by adjusting not only the VFe volume fraction of the hard/soft phases but also their arrangement.
UR - http://www.scopus.com/inward/record.url?scp=85147539784&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=85147539784&partnerID=8YFLogxK
U2 - 10.1063/9.0000506
DO - 10.1063/9.0000506
M3 - Article
AN - SCOPUS:85147539784
SN - 2158-3226
VL - 13
JO - AIP Advances
JF - AIP Advances
IS - 2
M1 - 025311
ER -