Pitting Corrosion Resistance of Ultrafine-Grained Aluminum Processed by Severe Plastic Deformation

In Joon Son, Hiroaki Nakano, Satoshi Oue, Shigeo Kobayashi, Hisaaki Fukushima, Zenji Horita

研究成果: ジャーナルへの寄稿記事

11 引用 (Scopus)

抄録

The effect of equal-channel angular pressing (ECAP) on the pitting corrosion resistance of Al and Al-Mg alloy was investigated by means of polarization curves in solutions containing 300 ppm of Cl - and by surface analysis. The potentials for pitting corrosion of Al and Al-Mg alloy were evidently shifted to the noble direction by ECAP process, indicating that this process improves resistance to pitting corrosion. SEM observation revealed that the pitting corrosion occurred near the impurity precipitates and the size of impurity precipitated decreased with ECAP process. The time-dependence of corrosion potential and the polarization resistance determined by AC impedance technique suggested that the formation rate of Al oxide films was increased with ECAP process. The improvement in pitting corrosion resistance of Al and Al-Mg by ECAP seems to be attributable to the decrease in the size of impurity precipitates and the increase in the formation rate of Al oxide films.

元の言語Japanese
ページ(範囲)892-898
ページ数7
ジャーナルNippon Kinzoku Gakkaishi/Journal of the Japan Institute of Metals
69
発行部数10
DOI
出版物ステータス出版済み - 10 1 2005

Fingerprint

Equal channel angular pressing
pitting
pressing
Pitting
Aluminum
corrosion resistance
plastic deformation
Corrosion resistance
Plastic deformation
aluminum
corrosion
Corrosion
Impurities
impurities
Oxide films
oxide films
Precipitates
precipitates
Polarization
Surface analysis

All Science Journal Classification (ASJC) codes

  • Condensed Matter Physics
  • Mechanics of Materials
  • Metals and Alloys
  • Materials Chemistry

これを引用

Pitting Corrosion Resistance of Ultrafine-Grained Aluminum Processed by Severe Plastic Deformation. / Son, In Joon; Nakano, Hiroaki; Oue, Satoshi; Kobayashi, Shigeo; Fukushima, Hisaaki; Horita, Zenji.

:: Nippon Kinzoku Gakkaishi/Journal of the Japan Institute of Metals, 巻 69, 番号 10, 01.10.2005, p. 892-898.

研究成果: ジャーナルへの寄稿記事

@article{f8a2a5fcaa714848a70de48456809910,
title = "Pitting Corrosion Resistance of Ultrafine-Grained Aluminum Processed by Severe Plastic Deformation",
abstract = "The effect of equal-channel angular pressing (ECAP) on the pitting corrosion resistance of Al and Al-Mg alloy was investigated by means of polarization curves in solutions containing 300 ppm of Cl - and by surface analysis. The potentials for pitting corrosion of Al and Al-Mg alloy were evidently shifted to the noble direction by ECAP process, indicating that this process improves resistance to pitting corrosion. SEM observation revealed that the pitting corrosion occurred near the impurity precipitates and the size of impurity precipitated decreased with ECAP process. The time-dependence of corrosion potential and the polarization resistance determined by AC impedance technique suggested that the formation rate of Al oxide films was increased with ECAP process. The improvement in pitting corrosion resistance of Al and Al-Mg by ECAP seems to be attributable to the decrease in the size of impurity precipitates and the increase in the formation rate of Al oxide films.",
author = "Son, {In Joon} and Hiroaki Nakano and Satoshi Oue and Shigeo Kobayashi and Hisaaki Fukushima and Zenji Horita",
year = "2005",
month = "10",
day = "1",
doi = "10.2320/jinstmet.69.892",
language = "Japanese",
volume = "69",
pages = "892--898",
journal = "Nippon Kinzoku Gakkaishi/Journal of the Japan Institute of Metals",
issn = "0021-4876",
publisher = "公益社団法人 日本金属学会",
number = "10",

}

TY - JOUR

T1 - Pitting Corrosion Resistance of Ultrafine-Grained Aluminum Processed by Severe Plastic Deformation

AU - Son, In Joon

AU - Nakano, Hiroaki

AU - Oue, Satoshi

AU - Kobayashi, Shigeo

AU - Fukushima, Hisaaki

AU - Horita, Zenji

PY - 2005/10/1

Y1 - 2005/10/1

N2 - The effect of equal-channel angular pressing (ECAP) on the pitting corrosion resistance of Al and Al-Mg alloy was investigated by means of polarization curves in solutions containing 300 ppm of Cl - and by surface analysis. The potentials for pitting corrosion of Al and Al-Mg alloy were evidently shifted to the noble direction by ECAP process, indicating that this process improves resistance to pitting corrosion. SEM observation revealed that the pitting corrosion occurred near the impurity precipitates and the size of impurity precipitated decreased with ECAP process. The time-dependence of corrosion potential and the polarization resistance determined by AC impedance technique suggested that the formation rate of Al oxide films was increased with ECAP process. The improvement in pitting corrosion resistance of Al and Al-Mg by ECAP seems to be attributable to the decrease in the size of impurity precipitates and the increase in the formation rate of Al oxide films.

AB - The effect of equal-channel angular pressing (ECAP) on the pitting corrosion resistance of Al and Al-Mg alloy was investigated by means of polarization curves in solutions containing 300 ppm of Cl - and by surface analysis. The potentials for pitting corrosion of Al and Al-Mg alloy were evidently shifted to the noble direction by ECAP process, indicating that this process improves resistance to pitting corrosion. SEM observation revealed that the pitting corrosion occurred near the impurity precipitates and the size of impurity precipitated decreased with ECAP process. The time-dependence of corrosion potential and the polarization resistance determined by AC impedance technique suggested that the formation rate of Al oxide films was increased with ECAP process. The improvement in pitting corrosion resistance of Al and Al-Mg by ECAP seems to be attributable to the decrease in the size of impurity precipitates and the increase in the formation rate of Al oxide films.

UR - http://www.scopus.com/inward/record.url?scp=29044439219&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=29044439219&partnerID=8YFLogxK

U2 - 10.2320/jinstmet.69.892

DO - 10.2320/jinstmet.69.892

M3 - 記事

AN - SCOPUS:29044439219

VL - 69

SP - 892

EP - 898

JO - Nippon Kinzoku Gakkaishi/Journal of the Japan Institute of Metals

JF - Nippon Kinzoku Gakkaishi/Journal of the Japan Institute of Metals

SN - 0021-4876

IS - 10

ER -