抄録
Rutile films were deposited on poly-1-lactide (PLLA) substrates using 0.5 M titanium tetrachloride aqueous solution at 40°C for 72 h. The rutile films exhibited excellent in vitro bioactivity as they induced apatite deposition in a simulated body fluid (SBF) within 3 days. This simple treatment provided an effective route to synthesize bioactive and biodegradable scaffolds.
本文言語 | 英語 |
---|---|
ページ(範囲) | 687-690 |
ページ数 | 4 |
ジャーナル | Key Engineering Materials |
巻 | 330-332 I |
DOI | |
出版ステータス | 出版済み - 1月 1 2007 |
外部発表 | はい |
!!!All Science Journal Classification (ASJC) codes
- 材料科学(全般)
- 材料力学
- 機械工学