We have synthesized single crystalline Ba 8Al xSi x-46 clathrates by using the flux Czochralski (CZ) method with Al-rich melt. The specific electric resistivity, the Seebeck coefficient and the power factor of single crystalline Ba 8Al 14Si 32 were 0.73 mΩcm, 70.0μV/K and 6.8×10 -4V 2/K 2Ωm, respectively. These values are higher than that of single crystalline Ba 8Al 12Si 34clathrate because of the reduced carrier concentration. It is indicated that Al contents and the carrier concentration of single crystalline Ba 8Al xSi 46-x can be controlled by using the flux Czochralski method.

元の言語英語
ホスト出版物のタイトルEnergy Harvesting - Recent Advances in Materials, Devices and Applications
ページ131-135
ページ数5
DOI
出版物ステータス出版済み - 1 1 2012
イベント2011 MRS Spring Meeting - San Francisco, CA, 米国
継続期間: 4 25 20114 29 2011

出版物シリーズ

名前Materials Research Society Symposium Proceedings
1325
ISSN(印刷物)0272-9172

その他

その他2011 MRS Spring Meeting
米国
San Francisco, CA
期間4/25/114/29/11

Fingerprint

Crystal growth from melt
Czochralski method
clathrates
Crystallization
crystallization
Fluxes
Crystalline materials
Seebeck effect
Carrier concentration
electrical resistivity
Seebeck coefficient
Electric conductivity

All Science Journal Classification (ASJC) codes

  • Materials Science(all)
  • Condensed Matter Physics
  • Mechanics of Materials
  • Mechanical Engineering

これを引用

Nakakohara, Y., Mugita, N., Nagatomo, Y., Saisho, M., Motooka, T., Teranishi, R., & Munetoh, S. (2012). Single crystallization of Ba 8Al xSi 46-x clathrate by using the flux Czochralski method. : Energy Harvesting - Recent Advances in Materials, Devices and Applications (pp. 131-135). (Materials Research Society Symposium Proceedings; 巻数 1325). https://doi.org/10.1557/opl.2011.1060

Single crystallization of Ba 8Al xSi 46-x clathrate by using the flux Czochralski method. / Nakakohara, Yusuke; Mugita, Naoki; Nagatomo, Yuya; Saisho, Makoto; Motooka, Teruaki; Teranishi, Ryo; Munetoh, Shinji.

Energy Harvesting - Recent Advances in Materials, Devices and Applications. 2012. p. 131-135 (Materials Research Society Symposium Proceedings; 巻 1325).

研究成果: 著書/レポートタイプへの貢献会議での発言

Nakakohara, Y, Mugita, N, Nagatomo, Y, Saisho, M, Motooka, T, Teranishi, R & Munetoh, S 2012, Single crystallization of Ba 8Al xSi 46-x clathrate by using the flux Czochralski method. : Energy Harvesting - Recent Advances in Materials, Devices and Applications. Materials Research Society Symposium Proceedings, 巻. 1325, pp. 131-135, 2011 MRS Spring Meeting, San Francisco, CA, 米国, 4/25/11. https://doi.org/10.1557/opl.2011.1060
Nakakohara Y, Mugita N, Nagatomo Y, Saisho M, Motooka T, Teranishi R その他. Single crystallization of Ba 8Al xSi 46-x clathrate by using the flux Czochralski method. : Energy Harvesting - Recent Advances in Materials, Devices and Applications. 2012. p. 131-135. (Materials Research Society Symposium Proceedings). https://doi.org/10.1557/opl.2011.1060
Nakakohara, Yusuke ; Mugita, Naoki ; Nagatomo, Yuya ; Saisho, Makoto ; Motooka, Teruaki ; Teranishi, Ryo ; Munetoh, Shinji. / Single crystallization of Ba 8Al xSi 46-x clathrate by using the flux Czochralski method. Energy Harvesting - Recent Advances in Materials, Devices and Applications. 2012. pp. 131-135 (Materials Research Society Symposium Proceedings).
@inproceedings{719026e3469c4faab22990de9db3b9c2,
title = "Single crystallization of Ba 8Al xSi 46-x clathrate by using the flux Czochralski method",
abstract = "We have synthesized single crystalline Ba 8Al xSi x-46 clathrates by using the flux Czochralski (CZ) method with Al-rich melt. The specific electric resistivity, the Seebeck coefficient and the power factor of single crystalline Ba 8Al 14Si 32 were 0.73 mΩcm, 70.0μV/K and 6.8×10 -4V 2/K 2Ωm, respectively. These values are higher than that of single crystalline Ba 8Al 12Si 34clathrate because of the reduced carrier concentration. It is indicated that Al contents and the carrier concentration of single crystalline Ba 8Al xSi 46-x can be controlled by using the flux Czochralski method.",
author = "Yusuke Nakakohara and Naoki Mugita and Yuya Nagatomo and Makoto Saisho and Teruaki Motooka and Ryo Teranishi and Shinji Munetoh",
year = "2012",
month = "1",
day = "1",
doi = "10.1557/opl.2011.1060",
language = "English",
isbn = "9781605113029",
series = "Materials Research Society Symposium Proceedings",
pages = "131--135",
booktitle = "Energy Harvesting - Recent Advances in Materials, Devices and Applications",

}

TY - GEN

T1 - Single crystallization of Ba 8Al xSi 46-x clathrate by using the flux Czochralski method

AU - Nakakohara, Yusuke

AU - Mugita, Naoki

AU - Nagatomo, Yuya

AU - Saisho, Makoto

AU - Motooka, Teruaki

AU - Teranishi, Ryo

AU - Munetoh, Shinji

PY - 2012/1/1

Y1 - 2012/1/1

N2 - We have synthesized single crystalline Ba 8Al xSi x-46 clathrates by using the flux Czochralski (CZ) method with Al-rich melt. The specific electric resistivity, the Seebeck coefficient and the power factor of single crystalline Ba 8Al 14Si 32 were 0.73 mΩcm, 70.0μV/K and 6.8×10 -4V 2/K 2Ωm, respectively. These values are higher than that of single crystalline Ba 8Al 12Si 34clathrate because of the reduced carrier concentration. It is indicated that Al contents and the carrier concentration of single crystalline Ba 8Al xSi 46-x can be controlled by using the flux Czochralski method.

AB - We have synthesized single crystalline Ba 8Al xSi x-46 clathrates by using the flux Czochralski (CZ) method with Al-rich melt. The specific electric resistivity, the Seebeck coefficient and the power factor of single crystalline Ba 8Al 14Si 32 were 0.73 mΩcm, 70.0μV/K and 6.8×10 -4V 2/K 2Ωm, respectively. These values are higher than that of single crystalline Ba 8Al 12Si 34clathrate because of the reduced carrier concentration. It is indicated that Al contents and the carrier concentration of single crystalline Ba 8Al xSi 46-x can be controlled by using the flux Czochralski method.

UR - http://www.scopus.com/inward/record.url?scp=84055221958&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84055221958&partnerID=8YFLogxK

U2 - 10.1557/opl.2011.1060

DO - 10.1557/opl.2011.1060

M3 - Conference contribution

AN - SCOPUS:84055221958

SN - 9781605113029

T3 - Materials Research Society Symposium Proceedings

SP - 131

EP - 135

BT - Energy Harvesting - Recent Advances in Materials, Devices and Applications

ER -