抄録
[(Fe0.5Co0.5)0.75B0.20 Si0.05]96Nb4 soft magnetic bulk metallic glasses were prepared by fluxing and water-quenching in a silica tube. Dimension of the bulk metallic glass specimens was up to 7.7 mm in diameter, which is about 1.5 times larger than those prepared by Cu mold-casting. The critical cooling rate of [(Fe0.5 Co0.5)0.75B0.20 Si0.05]96Nb4 alloys with fluxing for forming a metallic glass phase was 150 - 170 K/s, which was considerably smaller than that without fluxing. Saturation magnetization was 1.13 T, and coercivity was lower than 20 A/m. Fluxing suppresses heterogeneous nucleation by isolating the nucleation sites from the molten alloys and improves their glass-forming ability.
本文言語 | 英語 |
---|---|
ページ(範囲) | 126-130 |
ページ数 | 5 |
ジャーナル | Reviews on Advanced Materials Science |
巻 | 18 |
号 | 2 |
出版ステータス | 出版済み - 6月 2008 |
外部発表 | はい |
!!!All Science Journal Classification (ASJC) codes
- 材料科学(全般)
- 凝縮系物理学