抄録

A series of eight aliphatic polycarbonate (PC) glycols with various methylene numbers (HO-[(CH2)mOC(=O)O]2) m-OH, m = 3, 4, 5, 6, 7, 8, 9, and 10) were employed as a soft segment for a synthesis of polyurethane elastomers (PUEs). First of all, viscosity, glass transition temperature, melting point, and crystalline structure of these new PC-glycols were investigated. The PC-glycol-based PUEs were synthesized using the PC-glycols, 4,4′-diphenylmethane diisocyanate, and 1,4-butanediol by a one-shot method. Differential scanning calorimetry and small-angle X-ray scattering measurements revealed that the degree of microphase separation of the PC-glycol-based PUEs became first weaker and then stronger with increasing number of methylene groups of PC-glycols. The threshold carbon number for the degree of microphase separation was six. In the tensile testing, Young's modulus of the PUEs decreased and increased with an increase in the methylene number, which can be explained by the degree of microphase separation. Tensile strength and elongation at break of the PC-glycol-based PUEs increased and decreased with increasing the number of methylene groups. These results are associated with the ease of packing of the PC-glycol chains.

元の言語英語
ページ(範囲)8322-8327
ページ数6
ジャーナルMacromolecules
42
発行部数21
DOI
出版物ステータス出版済み - 11 10 2009
外部発表Yes

Fingerprint

polycarbonate
Elastomers
Glycols
Urethane
Polycarbonates
Polyurethanes
Mechanical properties
Microphase separation
Tensile testing
X ray scattering

All Science Journal Classification (ASJC) codes

  • Organic Chemistry
  • Materials Chemistry
  • Polymers and Plastics
  • Inorganic Chemistry

これを引用

Structure-mechanical property relationships for polycarbonate urethane elastomers with novel soft segments. / Kojio, Ken; Furukawa, Mutsuhisa; Motokucho, Suguru; Shimada, Makoto; Sakai, Machiko.

:: Macromolecules, 巻 42, 番号 21, 10.11.2009, p. 8322-8327.

研究成果: ジャーナルへの寄稿記事

Kojio, Ken ; Furukawa, Mutsuhisa ; Motokucho, Suguru ; Shimada, Makoto ; Sakai, Machiko. / Structure-mechanical property relationships for polycarbonate urethane elastomers with novel soft segments. :: Macromolecules. 2009 ; 巻 42, 番号 21. pp. 8322-8327.
@article{d62de90b8283421ba4466577b63ebeef,
title = "Structure-mechanical property relationships for polycarbonate urethane elastomers with novel soft segments",
abstract = "A series of eight aliphatic polycarbonate (PC) glycols with various methylene numbers (HO-[(CH2)mOC(=O)O]2) m-OH, m = 3, 4, 5, 6, 7, 8, 9, and 10) were employed as a soft segment for a synthesis of polyurethane elastomers (PUEs). First of all, viscosity, glass transition temperature, melting point, and crystalline structure of these new PC-glycols were investigated. The PC-glycol-based PUEs were synthesized using the PC-glycols, 4,4′-diphenylmethane diisocyanate, and 1,4-butanediol by a one-shot method. Differential scanning calorimetry and small-angle X-ray scattering measurements revealed that the degree of microphase separation of the PC-glycol-based PUEs became first weaker and then stronger with increasing number of methylene groups of PC-glycols. The threshold carbon number for the degree of microphase separation was six. In the tensile testing, Young's modulus of the PUEs decreased and increased with an increase in the methylene number, which can be explained by the degree of microphase separation. Tensile strength and elongation at break of the PC-glycol-based PUEs increased and decreased with increasing the number of methylene groups. These results are associated with the ease of packing of the PC-glycol chains.",
author = "Ken Kojio and Mutsuhisa Furukawa and Suguru Motokucho and Makoto Shimada and Machiko Sakai",
year = "2009",
month = "11",
day = "10",
doi = "10.1021/ma901317t",
language = "English",
volume = "42",
pages = "8322--8327",
journal = "Macromolecules",
issn = "0024-9297",
publisher = "American Chemical Society",
number = "21",

}

TY - JOUR

T1 - Structure-mechanical property relationships for polycarbonate urethane elastomers with novel soft segments

AU - Kojio, Ken

AU - Furukawa, Mutsuhisa

AU - Motokucho, Suguru

AU - Shimada, Makoto

AU - Sakai, Machiko

PY - 2009/11/10

Y1 - 2009/11/10

N2 - A series of eight aliphatic polycarbonate (PC) glycols with various methylene numbers (HO-[(CH2)mOC(=O)O]2) m-OH, m = 3, 4, 5, 6, 7, 8, 9, and 10) were employed as a soft segment for a synthesis of polyurethane elastomers (PUEs). First of all, viscosity, glass transition temperature, melting point, and crystalline structure of these new PC-glycols were investigated. The PC-glycol-based PUEs were synthesized using the PC-glycols, 4,4′-diphenylmethane diisocyanate, and 1,4-butanediol by a one-shot method. Differential scanning calorimetry and small-angle X-ray scattering measurements revealed that the degree of microphase separation of the PC-glycol-based PUEs became first weaker and then stronger with increasing number of methylene groups of PC-glycols. The threshold carbon number for the degree of microphase separation was six. In the tensile testing, Young's modulus of the PUEs decreased and increased with an increase in the methylene number, which can be explained by the degree of microphase separation. Tensile strength and elongation at break of the PC-glycol-based PUEs increased and decreased with increasing the number of methylene groups. These results are associated with the ease of packing of the PC-glycol chains.

AB - A series of eight aliphatic polycarbonate (PC) glycols with various methylene numbers (HO-[(CH2)mOC(=O)O]2) m-OH, m = 3, 4, 5, 6, 7, 8, 9, and 10) were employed as a soft segment for a synthesis of polyurethane elastomers (PUEs). First of all, viscosity, glass transition temperature, melting point, and crystalline structure of these new PC-glycols were investigated. The PC-glycol-based PUEs were synthesized using the PC-glycols, 4,4′-diphenylmethane diisocyanate, and 1,4-butanediol by a one-shot method. Differential scanning calorimetry and small-angle X-ray scattering measurements revealed that the degree of microphase separation of the PC-glycol-based PUEs became first weaker and then stronger with increasing number of methylene groups of PC-glycols. The threshold carbon number for the degree of microphase separation was six. In the tensile testing, Young's modulus of the PUEs decreased and increased with an increase in the methylene number, which can be explained by the degree of microphase separation. Tensile strength and elongation at break of the PC-glycol-based PUEs increased and decreased with increasing the number of methylene groups. These results are associated with the ease of packing of the PC-glycol chains.

UR - http://www.scopus.com/inward/record.url?scp=70449397324&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=70449397324&partnerID=8YFLogxK

U2 - 10.1021/ma901317t

DO - 10.1021/ma901317t

M3 - Article

VL - 42

SP - 8322

EP - 8327

JO - Macromolecules

JF - Macromolecules

SN - 0024-9297

IS - 21

ER -